TY - JOUR
T1 - Burst capacity analysis of pipeline with multiple longitudinally aligned interacting corrosion defects subjected to internal pressure and axial compressive stress
AU - Arumugam, Thibankumar
AU - Mohamad Rosli, Muhammad Kasyful Azhim
AU - Karuppanan, Saravanan
AU - Ovinis, Mark
AU - Lo, Michael
N1 - Publisher Copyright:
© 2020, Springer Nature Switzerland AG.
PY - 2020/7
Y1 - 2020/7
KW - Axial compressive stress
KW - Finite element analysis
KW - Internal pressure
KW - Multiple corrosion defect
KW - Pipe corrosion
UR - http://www.scopus.com/inward/record.url?scp=85100738967&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85100738967&partnerID=8YFLogxK
U2 - 10.1007/s42452-020-2994-7
DO - 10.1007/s42452-020-2994-7
M3 - Article
AN - SCOPUS:85100738967
SN - 2523-3971
VL - 2
JO - SN Applied Sciences
JF - SN Applied Sciences
IS - 7
M1 - 1201
ER -